Failure analysis of a crusher jaw
Plate 10.2 shows the macrostructure of a fractured surface along the teeth. The structure shows the features of brittle fractures. Plate 10.3 shows the optical micrograph of specimen taken from a failed crusher jaw. The microstructure is showing an austenitic structure with a feature of a structure around the grain boundaries and in the grains.